Chevron Phillips EB6025 HIPS - High Impact Polystyrene
Subcategory: Polystyrene; Thermoplastic
Material Notes: Rubber modified high impact polystyrene.Applications: - Cosmetic packaging
- Shower surrounds
- Point of purchase displays
- Thin-wall injection molding and thermoforming
Features:- Smooth, glossy surface finish
- Good durability
- High impact and stiffness
- Excellent toughness
Information provided by Chevron Phillips
| Available Properties |
- Specific Gravity
- Bulk Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |