| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Flexural Strength
- Impact Test
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Gloss
- Transmission, Visible
- Mold Temperature
|
|
|
|