Bapolene® Grade HD2032 HDPE, Blow Molding Resin
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Key Words: Excellent ESCR
Material Notes: Bapolene HD2032 is a high density polyethylene copolymer for blow molding applications. It is recommended for heavy duty applications that require excellent ESCR properties. This product meets the Food and Drug Administration requirements of 21CFR177.1520. Applications: General purpose blow molding, chemicals and detergents. Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers.
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|