Bapolene® Grade HD3252 Polyethylene, Injection Grade
Subcategory: Polyethylene; Thermoplastic; HDPE; Polymer
Key Words: Excellent impact strength, ESCR properties, and resistance to warpage
Material Notes: Narrow molecular weight distribution injection molding resin. This resin offers excellent impact strength, ESCR properties, and resistance to warpage. This product meets the Food and Drug Administration requirements of 21CFR177.1520. Applications: Containers, pails, industrial parts. All data is based upon injection-molded plaques. THIS PRODUCT DATA SHEET EFFECTIVE MARCH 2008 SUPERCEDES ALL DATA PREVIOUSLY PUBLISHED.
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Vicat Softening Point
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|