Bapolene® Grade LL3039 NAT Polyethylene, Rotational Molding Grade
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Key Words: Excellent environmental stress cracking resistance, warp resistance, and impact strength
Material Notes: Bapolene LL3039 is an LLDPE resin specifically designed for rotational molding applications. It offers excellent environmental stress cracking resistance, warp resistance, and impact strength. It is available in pellet or powder form. UV stabilized. This product meets FDA standards for food contact applications. Applications: Large rotational molded parts such as industrial and agricultural outdoor storage tanks, drums, and trash cans. Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Impact Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|