Bapolene® Grade PP4012 Polypropylene, Extrusion Grade
Subcategory: Polypropylene; Thermoplastic; Polymer
Key Words: Excellent stiffness and processability, chemical resistance, and ESCR properties
Material Notes: Bapolene PP4012 is a general purpose extrusion resin with excellent stiffness and processability, chemical resistance, and ESCR properties. This product meets FDA standards for food contact applications. Applications: Sheet, profile, pipe, and strapping. Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
| Available Properties |
- Density
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|