Bapolan® Grade PS6080 General Purpose Polystyrene Injection Molding Resin
Subcategory: Polystyrene; Thermoplastic; Polymer
Key Words: Excellent clarity and cycle time
Material Notes: Type: High flow general purpose injection molding resin. This resin offers excellent clarity and cycle time.This resin meets FDA requirements. Applications: Houseware, packaging, novelties, disposable cutlery, disposable tumblers, and other small or thin wall molding. Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers.