Bapolene® Grade LL122B Polyethylene, Film Grade
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Key Words: Excellent tensile and toughness properties
Material Notes: Bapolene LL122B is a general purpose LLDPE for blown film extrusion. This resin offers excellent tensile and toughness properties. Contains no slip and no antiblock additives. This product meets FDA standards for food contact applications. Applications: Industrial bags, shipping sacks, frozen food packaging, trash bags. Film properties are based on a thickness of 1.0 mil, blow-up ratio of 2.5:1 and 0.1 mm/mm-min Initial Strain Rate. Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- 1% Secant Modulus, MD
- 1% Secant Modulus, TD
- Haze
- Gloss
- Process
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|