Durez® 18441 Phenolic, Compression Grade
Subcategory: Phenolic; Thermoset
Close Analogs: Data is also available in MatWeb for injection molding grade. Data provided by the manufacturer.
Material Notes: Durez 18441 Black Phenolic is a single-stage, electrical grade molding material. It is recommended for electrical applications such as switch cases, coil forms., terminal plates, etc. where absence of ammonia out gassing is required to prevent corrosion of metal contacts. Due to its CTI of 180V, it is also recommended for wiring devices (damp and wet locations).
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|