Durez® 30725 Phenolic, Compression Grade
Subcategory: Phenolic; Thermoset
Close Analogs: Data is also available in MatWeb for injection molding grade. Data provided by the manufacturer.
Material Notes: Durez 30725 Black Phenolic is a two stage, general purpose molding material with a Tracking Index of 175+ volts. It is recommended for wiring device applications.
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|