Durez® 31735 Phenolic, Injection Grade
Subcategory: Phenolic; Thermoset
Close Analogs: Data is also available in MatWeb for compression molding grade. Data provided by the manufacturer.
Material Notes: Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimensional tolerance, impact strength, and other properties required in pulley applications.
| Available Properties |
- Density
- Apparent Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Poissons Ratio
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|