Sumikon® PM-9501 Glass-Filled Phenolic, Compression Grade
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: Data is also available in MatWeb for injection molding grade. Data provided by the manufacturer.
Material Notes: Sumikon® PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional stability with excellent heat resistance. Typical applications include brush holders, housings, and heat insulators.
| Available Properties |
- Specific Gravity
- Bulk Density
- Bulk Factor
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|