Durez® 30190 Glass-Filled Phenolic, Compression Grade
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: Data provided by the manufacturer.
Material Notes: Durez 30190 Brown Phenolic is a two-stage, mineral and glass filled, special purpose molding material. It is formulated for applications requiring good dimensional stability and high heat resistance.
| Available Properties |
- Specific Gravity
- Bulk Density
- Bulk Factor
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|