FM 1132P Cellulose Reinforced Phenolic Novolac
Subcategory: Phenolic; Thermoset; Polymer
Close Analogs: Former Rogers & Vyncolit North America products are now manufactured by Sumitomo Bakelite North America.
Material Notes: FM 1132P is a two-stage phenolic molding compound reinforced with cellulose in pellet form. FM-1132P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-10. (Replaces Military Specification MIL-M-14H.) Information supplied by Sumitomo Bakelite North America.
| Available Properties |
- Density
- Bulk Density
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell E
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Dielectric Strength
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Available Molding Grades
- Color
- Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|