Solvay Advanced Polymers Udel® GF-130 Polysulfone
Subcategory: Polysulfone; Thermoplastic
Close Analogs: This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.
Material Notes:
Data provided by the manufacturer, Amoco Corporation. A tough, rigid, high-strength amorphous thermoplastic that maintains its properties over a wide temperature range. Good electrical properties, clarity and toughness, plus exceptional steam resistance.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Tensile Impact Strength
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|