Solvay Advanced Polymers Kadel® E-1230 Polyketone
Subcategory: Polyketone; Thermoplastic
Close Analogs: This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.
Material Notes:
Data provided by the manufacturer, Amoco Corporation. Electrical Conductor. High performance proprietary semi-crystalline polymer based resins with exceptional solvent resistance and high temperature performance. They provide strength and stiffness, plus superior chemical resistance for application in hostile environments.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Tensile Impact Strength
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|