Solvay Advanced Polymers AMODEL® A-1133 HS Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded

 

Subcategory: Polyphthalamide; Thermoplastic; Polymer

Material Notes:
AMODEL A-1133 HS resin is a 33% glass reinforced heat stabilized polyphthalamide (PPA) which exhibits a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin, and it can be easily processed using conventional equipment and methods.

Information provided by Solvay Advanced Polymers

Available Properties
  • Specific Gravity
  • Moisture Absorption at Equilibrium
  • Hardness, Rockwell R
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break at Elevated Temperature
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Compressive Strength
  • Poissons Ratio
  • Shear Strength
  • Izod Impact, Notched (ISO)
  • Izod Impact, Unnotched
  • Izod Impact, Unnotched (ISO)
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Izod Impact, Notched
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • High Voltage Arc Resistance to Ignition (HVAR)
  • Comparative Tracking Index
  • CTE, linear 100°C
  • CTE, linear 250°C
  • Melting Point
  • Maximum Service Temperature, Air
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flammability, UL94
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。