Solvay Advanced Polymers AMODEL® A-1133 HS Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
Subcategory: Polyphthalamide; Thermoplastic; Polymer
Material Notes: AMODEL A-1133 HS resin is a 33% glass reinforced heat stabilized polyphthalamide (PPA) which exhibits a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance and low moisture absorption are also characteristic of this resin, and it can be easily processed using conventional equipment and methods.Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell R
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Poissons Ratio
- Shear Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Unnotched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- High Voltage Arc Resistance to Ignition (HVAR)
- Comparative Tracking Index
- CTE, linear 100°C
- CTE, linear 250°C
- Melting Point
- Maximum Service Temperature, Air
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|