Solvay Advanced Polymers AMODEL® AS-1566 HS Polyphthalamide (PPA) Resin, 65% Glass and Mineral Reinforced, Dry as Molded
Subcategory: Polyphthalamide; Thermoplastic; Polymer
Material Notes: AMODEL AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin which exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically to be cost effective for most applications requiring high stiffness, good dimensional stability, chemical resistance, and toughness. The material is readily processed using conventional injection molding equipment and methods. Potential applications for AMODEL AS-1566 HS resin include electrical connectors and housings, motor components, pistons, covers, and engine and transmission components. Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Shear Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Unnotched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- CTE, linear 100°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|