Solvay Advanced Polymers AMODEL® A-1565 HS Polyphthalamide (PPA) Resin, 65% Glass and Mineral Reinforced, Dry as Molded
Subcategory: Polyphthalamide; Thermoplastic; Polymer
Material Notes: AMODEL A-1565 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) which exhibits a high deflection temperature and flexural modulus. This grade was designed specifically to be cost effective in applications requiring high stiffness, good dimensional stability, and good retention of stiffness at elevated temperatures. The material can be easily processed using conventional injection molding equipment and methods. Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Shear Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Unnotched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- Volume Resistivity
- High Voltage Arc Resistance to Ignition (HVAR)
- Comparative Tracking Index
- CTE, linear 100°C
- CTE, linear 250°C
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|