Solvay Advanced Polymers AMODEL® A-1240 L Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
Subcategory: Polyphthalamide; Thermoplastic; Polymer
Material Notes: AMODEL® A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent dimensional stability and low moisture absorption. There are two versions of AMODEL A-1240 resin, “L” and “HS”. The L version will usually provide the smoother, higher gloss surface, while the HS version gives better long-term thermal aging properties. Both AMODEL A-1240 resins can be easily processed using conventional equipment and methods. Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell R
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Poissons Ratio
- Shear Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Unnotched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dissipation Factor
- High Voltage Arc Resistance to Ignition (HVAR)
- Comparative Tracking Index
- CTE, linear 100°C
- CTE, linear 250°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|