Solvay Advanced Polymers AMODEL® FR-4133 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, Dry as Molded
Subcategory: Polyphthalamide; Thermoplastic; Polymer
Material Notes: AMODEL FR-4133 is a 33% glass-reinforced polyphthalamide (PPA) resin designed for electrical and electronic applications. This UL94-V0 resin offers the highest mechanical and electrical properties, plus superior thermal performance to resist blistering during lead-free SMT processes.
Color stability is enhanced compared to previous flame-retarded grades. Quick crystallization in water-cooled molds allows for fast cycle times using mold temperatures as low as 150°F (65°C). Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell R
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Shear Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Unnotched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Strength
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Amp Arc Ignition, HAI
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|