Solvay Advanced Polymers AMODEL® AT-6115 HS Polyphthalamide (PPA) Resin, 15% Glass Fiber Reinforced, Dry as Molded
Subcategory: Polyphthalamide; Thermoplastic; Polymer
Material Notes: AMODEL AT-6115 HS is a 15% glass-fiber reinforced toughened grade of polyphthalamide (PPA) resin that has more elongation than other 15% glass-fiber reinforced grades of AMODEL resin. This grade was developed for automotive snap-fit electronic connectors. This resin processes readily using conventional injection molding equipment and methods. It offers high flow and short molding cycles. The processing window is relatively broad, and mold temperatures as low as 150°F (65°C) can be used. Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Shear Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Unnotched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|