Solvay Advanced Polymers AMODEL® AT-1116 HS Polyphthalamide (PPA) Resin, 16% Glass Reinforced, Dry as Molded
Subcategory: Polyphthalamide; Thermoplastic; Polymer
Material Notes: AMODEL AT-1116 HS resin is a toughened polyphthalamide (PPA) grade containing 16% glass reinforcement. This resin has a high heat deflection temperature and a high flexural modulus with greater tensile elongation than standard untoughened glass reinforced grades of PPA. This grade was designed specifically to be cost effective for many applications requiring stiffness, good dimensional stability, chemical resistance and ductility. This material can be molded using conventional injection molding equipment and standard methods. Potential applications for AMODEL AT-1116 HS resin include bearings, bearing retainers/cages, housings, chemical process equipment components, motor frames, sporting equipment, lawn and garden equipment, and various applications requiring press-fit or snap-fit assembly. Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Shear Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Unnotched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Dynatup @ -18°C
- Dynatup @ -18°C Max Load
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|