Solvay Advanced Polymers AMODEL® ET-1001 L Polyphthalamide (PPA) Resin, Dry as Molded

 

Subcategory: Polyphthalamide; Thermoplastic

Material Notes:
AMODEL ET-1001 L resin is an impact modified polyphthalamide (PPA) with exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, and good chemical resistance combined with good mechanical property retention over a broad temperature/ humidity range.

Possible applications for AMODEL ET-1001 L resin include anti-friction and wear resistant components, and components of chemical and oil processing equipment, sporting goods, automobiles, household appliances, power tools, and safety equipment, where exceptional impact strength and high modulus are required.

AMODEL ET-1001 L resin contains a lubricant for easier processing with conventional equipment and methods.

Information provided by Solvay Advanced Polymers

Available Properties
  • Specific Gravity
  • Moisture Absorption at Equilibrium
  • Tensile Strength at Break
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Elongation at Break at Elevated Temperature
  • Elongation at Yield
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Poissons Ratio
  • Shear Strength
  • Izod Impact, Notched (ISO)
  • Izod Impact, Unnotched (ISO)
  • Charpy Impact Unnotched
  • Charpy Impact, Notched
  • Dynatup @ -18°C
  • Dynatup @ -18°C Max Load
  • Izod Impact, Notched
  • Melting Point
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。