Solvay Advanced Polymers AMODEL® ET-1000 HS Polyphthalamide (PPA) Resin, at 50% RH
Subcategory: Polyphthalamide; Thermoplastic
Material Notes: AMODEL ET-1000 HS is an impact modified polyphthalamide (PPA) which exhibits exceptional impact strength and practical toughness. AMODEL PPA resins offer high fatigue strength, good chemical resistance, and high mechanical property retention over a broad temperature and humidity range. AMODEL ET-1000 HS resin can be easily processed using conventional equipment and methods. Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Dynatup @ -18°C
- Izod Impact, Notched
- Melting Point
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|