Solvay Advanced Polymers AMODEL® A-6135 HN Polyphthalamide (PPA) Resin, 35% Glass Reinforced, Dry as Molded
Subcategory: Polyphthalamide; Thermoplastic; Polymer
Material Notes: AMODEL A-6135 HN polyphthalamide (PPA), a 35% glass reinforced resin, is one of the PPA resins designed to give high crystallinity when molded in water-cooled molds. Key properties of the resin are high heat resistance, high strength and stiffness over a broad temperature range, low moisture absorption, excellent chemical resistance, and excellent electrical properties. AMODEL A-6135 HN resin can be advantageously used for many automotive electrical and electronic applications. These applications may include connectors, sockets, switches, sensors, enclosures, and housings for systems, such as anti-lock brake, traction control, steering, electronic engine control, transmission control, and chassis controls. This material processes readily on conventional injection molding equipment using water-cooled molds. Its rapid crystallization rate and high flow can result in short cycles and therefore high molding productivity and lower part cost. Information provided by Solvay Advanced Polymers
| Available Properties |
- Specific Gravity
- Moisture Absorption at Equilibrium
- Hardness, Rockwell R
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break at Elevated Temperature
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Poissons Ratio
- Shear Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Izod Impact, Unnotched (ISO)
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Shrinkage
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|