Cytec Thornel® Carbon Fiber VCB-20 Carbon Cloth/Epoxy Composite
Subcategory: Epoxy; Thermoset; Carbon Fiber/Thermoset Composite; Polymer
Close Analogs: Thornel® products were sold by Amoco and are now owned by Cytec.
Key Words: Carbon Fibre; BP Amoco Performance Products
Material Notes: Data provided by the manufacturer, Amoco Performance Products, Inc. Cured ply 0.47 mm thick, 55% fiber vol.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- CTE, linear 20°C
|
|
|
|