Ebbtide Polymers 900 Transparent ABS
Subcategory: ABS Polymer; Thermoplastic
Key Words: MABS; Poly(Acylonitrile Butadiene Styrene)
Material Notes: Suitable for injection or extrusion. The property values below are typical data under specific test conditions and are not intended for product design use. Information provided by Ebbtide Polymers.
| Available Properties |
- Density
- Water Absorption
- Viscosity
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Izod Impact, Notched, Low Temp
- CTE, linear 20°C
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Transmission, Visible
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|