LANXESS Pocan® KL1-7341 PBT, 40% Glass Fiber/Mineral
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic; Polymer
Close Analogs: LANXESS was spun-off from Bayer in early 2005. This product is no longer listed as a standard NAFTA product.
Material Notes:
Characteristics: Thermoplastic (PET) Modified: Low Warpage Applications: Parts Requiring Good Surface and Low Warpage Processing: Injection Molding (Melt Temperature: 464-518°F, Mold Temperature: 160-250°F)
| Available Properties |
- Density
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Hardness, Rockwell R
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Arc Resistance
- Deflection Temperature at 1.8 MPa (264 psi)
- Processing Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|