Starex® HF-5330S ASA, Unreinforced
Subcategory: ASA Polymer; Thermoplastic
Material Notes: Amorphous Styrene Acrylonitrile (SAN) Characteristics: Heat Resistant: Impact and Chemical Resistance, Surface Gloss Applications: Oil Filter Case, Lubricant Can, Refrigerator and Hair Dryer Components Processing: Injection Molding (Melt Temperature: 460-500°F, Mold Temperature: 100-175°F) Starex® is a registered trademark of Cheil Industries, Inc.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Processing Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|