Starex® VH-0800 ABS, Unreinforced
Subcategory: ABS Polymer; Thermoplastic
Material Notes: Amorphous Acrylonitrile Butadiene Styrene (ABS) Characteristics: Flame Retardant: Balance of Properties (Impact, Mechanical and Heat) Applications: Computer, Monitor and Printer Housings, Microwave Components Processing: Injection Molding (Melt Temperature: 320-425°F, Mold Temperature: 100-140°F) Starex® is a registered trademark of Cheil Industries, Inc.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength at Break
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Processing Temperature
- Mold Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|