Abatron AboCast 8-7/Abocure 8-7 Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: 2-part solvent-free dielectric epoxy casting compound. Processing: 100/50 ratio (pbw); Gel time, 1 lb. (2.2 kg): 125 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F). Applications: solventless casting, adhesive, and coating.
| Available Properties |
- Water Absorption
- Viscosity Measurement
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Strength
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dissipation Factor
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|