Abatron AboCast 8-22/Abocure 8-22 Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: 2-part, clear, solvent-free dielectric epoxy casting compound. Processing: 100/55.00 ratio (pbw); Gel time, 100 g (3.5 oz.): 23 hours at 20°C (68°F). Applications: solventless casting, adhesive, and coating.