Abatron AboCast 50-16/AboCure 50-1 Epoxy
Subcategory: Epoxy; Thermoset
Key Words: potting, casting, encapsulating, impregnating
Material Notes: Information provided by Abatron, Inc. Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 380 min. at 25°C (77°F). Exothermic Peak 154°C (310°F). Hardens in 2-24 hours at RT (faster with heat). Full cure in 1-5 weeks at RT or 1-4 hrs at 80-120°C (175-250°F).
| Available Properties |
- Viscosity Measurement
- Hardness, Rockwell M
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Compressive Modulus
- Izod Impact, Notched
- Electrical Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Maximum Service Temperature, Air
- Pot Life
- Exotherm
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|