Abatron AboCast 8012-3/AboCure 8012-3 Epoxy
Subcategory: Epoxy; Thermoset
Key Words: potting, casting, encapsulating, impregnating
Material Notes: Data provided by the manufacturer, Abatron, Inc. Low-viscosity, Heavy-duty, Dark Amber color. Shelf life is 12+ months. Processing: 2/1 ratio. Pot life: 30 minutes.Corrosion Resistance Superior resistance to alkalis, organic acids, and water.Applications: Food and dairy plant floors.
| Available Properties |
- Hardness, Shore D
- Tensile Strength, Ultimate
- Compressive Yield Strength
- Maximum Service Temperature, Air
|
|
|
|