Abatron AboCast 8012-9/AboCure 8012-9 Epoxy
Subcategory: Epoxy; Thermoset
Key Words: potting, casting, encapsulating, impregnating
Material Notes: Data provided by the manufacturer, Abatron, Inc. 5-minute epoxy. Light Amber color, Medium viscosity. Not as brittle as conventional 5-minute epoxies. Fastest Abatron "VR" Epoxy with good physical and chemical properties. Popular in 1-ouce "MIXPAK" pouches. Shelf life is 12+ months. Processing: 1/1 ratio. Pot life: 5 minutes. Hardens even at 0°C (32°F).
| Available Properties |
- Hardness, Shore D
- Tensile Strength, Ultimate
- Compressive Yield Strength
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|