Abatron AboCast 8101-2/AboCure 8101-2 Epoxy
Subcategory: Epoxy; Thermoset
Key Words: potting, casting, encapsulating, impregnating
Material Notes: Data provided by the manufacturer, Abatron, Inc. Lower-viscosity than AboCast 8101-1 for easier casting, encapsulating and potting. Shelf life is 12+ months. Processing: 2-1 ratio. Pot life: 2-3 hrs. Full properties developed by heat cure or postcure.Applications: Best Abatron "VR" Epoxy combination of low viscosity, chemical, structural, thermal & dielectric properties for critical castings.
| Available Properties |
- Hardness, Shore D
- Tensile Strength, Ultimate
- Compressive Yield Strength
- Maximum Service Temperature, Air
|
|
|
|