Abatron AboCast/AboCure 8109-3
Subcategory: Epoxy; Thermoset
Material Notes: Low viscosity, RT cure. Easy processing. Processing: 100/10 pbw; Potlife: 2.5 h/20°C (68°F), 30 min/40°C (105°F), 15 min/60°C (140°F); mix at RT; cures in: 24 h/20°C (68°F), 2-3 h/60°C (140°F), 15 min/100°C (212°F). Applications: Laminating, small parts, and potting.
| Available Properties |
- Density
- Water Absorption
- Viscosity
- Vapor Pressure
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Compressive Yield Strength
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Processing Temperature
- Pot Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|