Abatron AboCast/AboCure 8109-5
Subcategory: Epoxy; Thermoset
Key Words: castings, laminating, laminates
Material Notes: High heat resistance. Easy to use. Processing: 100/20 pbw; Potlife: 7-10 days/20°C (68°F), 5-7h/60°C (140°F); mix at RT; cures in: 4 h/100°C (212°F) + 3 h/190°C (375°F) postcure. Applications: Castings and laminates for high temperature applications.
| Available Properties |
- Density
- Water Absorption
- Viscosity
- Vapor Pressure
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Compressive Yield Strength
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Processing Temperature
- Pot Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|