Abatron AboCast/AboCure 8109-10
Subcategory: Epoxy; Thermoset
Key Words: impregnating, composites, potting
Material Notes: 2-part, clear, slow casting/impregnating dielectric compound. Low dielectric constant, good flexibility and thermocycling properties. Abocast 8502-4 is a red (and other colors), filled version. Processing: 100% solids; 100/130 ratio; Potlife: 6-8 days/20°C (68°F); 1-2 days 40°C (105°F), 10-15 hours at 60°C (140°F); cures im: 8 h/80°C (175°F), 6 h/100°C (212°F), 4 h/120°C (250°F); mix thoroughly at RT, heat to desired viscosity, apply to clean, dry surface. Applications: Impregnating and potting.
| Available Properties |
- Density
- Water Absorption
- Viscosity
- Vapor Pressure
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Compressive Yield Strength
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Processing Temperature
- Pot Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|