Abatron AboCast/AboCure 8109-13
Subcategory: Epoxy; Thermoset
Key Words: potting, laminating, laminates
Material Notes: Liquid hardener version of AboCast/AboCure 8109-11. Processing: 100/23 pbw; Potlife: 3-5 h/20°C (68°F), 1-3 h/40°C (105°F), 0.5-1 h/60°C (140°F); mix at RT; cures in: 30 mins/60°C (140°F), 45 min/100°C (212°F), 30 mins/140°C (285°F), 15 min+1-3h/180°C (355°F). Applications: Potting and laminating.
| Available Properties |
- Density
- Water Absorption
- Viscosity
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Flexural Yield Strength
- Compressive Yield Strength
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Processing Temperature
- Pot Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|