Abatron AboWeld 8012-6/AboCure 8012-6 Epoxy
Subcategory: Epoxy; Thermoset
Key Words: potting, casting, encapsulating, impregnating
Material Notes: Data provided by the manufacturer, Abatron, Inc. Iron filled putty, "plastic steel". non-shrinking, adhesive filler. Shelf life is 12+ months. Processing: Pot life: 1-2 hrs. 2/1 ratio.Applications: All-purpose structural adhesive, high-strength filler and metal patching compound.
| Available Properties |
- Hardness, Shore D
- Tensile Strength, Ultimate
- Compressive Yield Strength
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|