Abatron AboWeld 8101-5/AboCure 8101-5 Epoxy
Subcategory: Epoxy; Thermoset
Key Words: potting, casting, encapsulating, impregnating
Material Notes: Data provided by the manufacturer, Abatron, Inc. 5-minute epoxy thixotropic paste. Vaseline like consistency of 8012-9. Light Amber color. Shelf life is 12+ months. Processing: 1/1 ratio. Pot life: 5-minutes. Non-runny, but light to mix.Applications: patches and filling in all-weather, emergency and difficult conditions.