Abatron AboWeld 8101-9/AboCure 8101-9 Epoxy
Subcategory: Epoxy; Thermoset
Key Words: potting, casting, encapsulating, impregnating
Material Notes: Data provided by the manufacturer, Abatron, Inc. Aluminum filled thixotropic paste. Highest heat, solvent and chemical resistance. Shelf life is 12+ months. Processing: Pot life: 1-2 hrs. 2/1 ratio. Full properties developed by heat cure or postcure. Highest grade "VR" metal-filled adhesive paste, filler and patching compound mainly for heat and chemical resistance.
| Available Properties |
- Hardness, Shore D
- Tensile Strength, Ultimate
- Compressive Yield Strength
- Maximum Service Temperature, Air
|
|
|
|