Abatron AboCast 4-4/AboCure 50-12 Casting Epoxy for Tooling
Subcategory: Epoxy; Thermoset
Material Notes: Standard casting compound for molds or patterns of any size, that can be machined with common metal working tools, engraving and reproduction molds. Main Advantages: - Fast
- Best rigid, chemical, and heat properties with room temperature cure
Main Drawbacks: - Too fast for thick castings (>1inch)
- Needs precise ratios
Processing: 100/5 ratio. Room temperature cure 2 to 8 hours, optional post-cure 2 to 4 hours at 80 to 120°C. Information provided by Abatron.
| Available Properties |
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- Flexural Strength
- Compressive Strength
- Thermal Conductivity
- Maximum Service Temperature, Air
- Pot Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|