Abatron KromaKote 8901-8 Polyurethane Coating
Subcategory: Polyurethane, TP; Thermoplastic
Material Notes: 2-component system for outstanding performance in normal, industrial, marine and corrosive environments. Superb combination of chemical, solvent, abrasion and weather resistance. Suggested Uses: Protective and decorative coating and resurfacing of tanks, tubs, sinks, tiles, appliances, metal panels, machinery, bulkheads, walls, counters, and all kinds of indoor and outdoor surfaces. Available in custom colors. Processing: Ratio by volume: 2 parts Kromakote 8901-8 Part A (colored resin solution) to 1 part Kromakote 8901-8 Part B (clear coreactant solution). Information provided by Abatron.
| Available Properties |
- Density
- Solids Content
- Volatile Organic Compounds (VOC) Content
- Viscosity
- Taber Abrasion, mg/1000 Cycles
- Pot Life
- Pencil Hardness
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|