Abatron AboThane 8003-3 Polyurethane Coating
Subcategory: Polyurethane, TP; Thermoplastic
Material Notes: AboThane 8003-3 is a clear one-package, moisture-cure polyurethane coating for hardwood, concrete and seamless floors. It was designed for high flexibility, excellent wear and antiskid properties, and abrasion, chemical and corrosion resistance. Suggested Uses: Floors in warehouses, factories, chemical and food processing plants, gymnasiums, laboratories, clinics, hospitals, classrooms, offices, stores, RR boxcars, seamless floors, aircraft and missile plants, homes and garages, restaurants, and etc. Information provided by Abatron.
| Available Properties |
- Density
- Solids Content
- Viscosity
- Film Elongation at Break, MD
- Impact Test
- Taber Abrasion, mg/1000 Cycles
- Film Tensile Strength at Break, MD
- Flash Point
- Gardner Color Number
- Dry Time
- Mandrel Flexibility
- Sward Hardness
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|