Abatron AboCast 50-7/AboCure 8501-4 High Temperature Resistant Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: Clear amber, high viscosity, structural/dielectric epoxy with high temperature resistance. Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to be used at temperatures up to 300°C. Casting and assembly of tools, patterns, models and structural components that must operate in extremely hot and corrosive environments. Processing: 100/89 ratio (pbw). Cured 2 hours at 95°C + 24 hour post-cure at 260°C. Information provided by Abatron.
| Available Properties |
- Viscosity
- Tensile Strength @ Break
- Flexural Strength
- Compressive Strength
- Thermal Conductivity
- Maximum Service Temperature, Air
- Pot Life
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|