Abatron AboCast 8501-6/AboCure 8501-4 High Temperature Resistant Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: 1-component system. Clear amber, low viscosity, structural/dielectric epoxy. Processing: Pot Life: 5-9 months. Cured 2 hours at 95°C + 15 hour post-cure at 230°C. Information provided by Abatron.
| Available Properties |
- Viscosity
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |